Title:
The New NRMCA Quality Certification Program
Author(s):
Obla, K.H., and Lobo, C.L.
Publication:
Concrete International
Volume:
36
Issue:
12
Appears on pages(s):
41-45
Keywords:
concrete, manual, management, production
DOI:
Date:
12/1/2014
Abstract:
A Quality Management System (QMS) can improve the quality of a company’s product by establishing a systematic way of setting quality processes and responsibilities. The NRMCA Quality Certification program was established to assure that ready mixed concrete companies have and follow a comprehensive QMS. This certification program can be used to pre-qualify concrete producers for high profile projects and for those projects with performance-based specifications. Criteria evaluated during the verification process for the NRMCA quality certification are highlighted.