Title:
Torsion, Bending, and Confusion-An Attempt to Establish the Facts
Author(s):
Paul Lampert and Michael P. Collins
Publication:
Journal Proceedings
Volume:
69
Issue:
8
Appears on pages(s):
500-504
Keywords:
Beams (supports), bending, building codes,
prestressed concrete, reinforced concrete, research, structural design
DOI:
10.14359/7163
Date:
8/1/1972
Abstract:
Attempts to clear confusion created by seemingly contradictory papers published about torsion in reinforced concrete members. Provides facts related to torsional strength and torsion-bending interaction behavior and gives simple design expressions.