Title: Green Concrete for Sustainable 3DCP

Author(s): Wilson Ricardo Leal da Silva and Martin Kaasgaard

Publication: Concrete International

Volume: 44

Issue: 4

Appears on pages(s): 34-40

Keywords: cement, aggregate, emission, composition

DOI:

Date: 4/1/2022

Abstract:
There is a need to further study mixtures for three-dimensional concrete printing (3DCP) that incorporate fractions of large aggregates to develop more robust composition and achieve a feedstock with lower embodied energy. The main scope of this article is the scaling up of the solid constituents in such 3DCP mixtures.