Title: Odense Robotics Collaboration Project

Author(s): Wilson Ricardo Leal da Silva and Roberto Naboni

Publication: Concrete International

Volume: 43

Issue: 9

Appears on pages(s): 30-31

Keywords: construction, automation, monitoring, system

Date: 9/1/2021

Abstract:
Extrusion-based, three-dimensional concrete printing (3DCP) is one of the main areas of development in architectural and construction robotics, however, the process remains characterized by limited levels of automation. To move 3DCP closer to a truly automated digital fabrication, a group of Danish researchers and companies established the 3DLOOP project.




  