SPEC-522.1-20: Specification for Construction of Pervious Concrete Pavement (SI Units)

Abstract:

This Specification covers minimum requirements for the construction of pervious concrete pavement. This Specification covers materials, preparation, forming, placing, finishing, jointing, curing, and quality control of pervious concrete pavement. Provisions governing testing, evaluation, and acceptance of pervious concrete pavement are included.