ACI PRC-544.5-10: Report on the Physical Properties and Durability of Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 3/2010 Price:$ 68.50 USD Become a Member More Info »
ACI PRC-544.6-15 Report on Design and Construction of Steel Fiber-Reinforced Concrete Elevated Slabs Topic: Fiber-Reinforced Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 9/2015 Price:$ 90.50 USD Become a Member More Info »
ACI PRC-544.8-16: Report on Indirect Method to Obtain Stress-Strain Response of Fiber-Reinforced Concrete (FRC) Topic: Fiber-Reinforced Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 4/2016 Price:$ 70.50 USD Become a Member More Info »
ACI PRC-544.2-17: Report on the Measurement of Fresh State Properties and Fiber Dispersion of Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 5/2017 Price:$ 54.50 USD Become a Member More Info »
COLUSB24: 2024 USB ACI Collection of Concrete Codes, Specifications, and Practices Format: Printed Document Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Technical Committees Published: 1/2024 Regular Price: $ 1,049.00 USD Member Price: $ 629.00 USD Become a Member More Info »
ACI PRC-544.1R-96: Report on Fiber Reinforced Concrete (Reapproved 2009) Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 9/2002 Price:$ 79.50 USD Become a Member More Info »
ACI Collection of Concrete Codes, Specifications, and Practices - 2024 Format: Printed Document Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Technical Committees Published: 1/2024 Regular Price: $ 1,299.00 USD Member Price: $ 799.00 USD Become a Member More Info »
ACI PRC-549.3-22: Glass Fiber-Reinforced Concrete Premix—Report Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 549 Published: 9/2022 Price:$ 54.00 USD Become a Member More Info »
ACI PRC-544.4-18: Guide to Design with Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: Printed Document or PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 7/2018 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-440.2-23: Design and Construction of Externally Bonded Fiber-Reinforced Polymer (FRP) Systems for Strengthening Concrete Structures—Guide Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 440 Published: 11/2023 Price:$ 99.00 USD Become a Member More Info »
SPEC-544.12-23: Performance-Based Fiber-Reinforced Concrete for Slabs-on-Ground and Overlays—Specification Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 544 Published: 12/2023 Regular Price: $ 54.00 USD Member Price: $ 34.00 USD Become a Member More Info »
ACI PRC-506.1-21: Fiber-Reinforced Shotcrete - Guide Topic: Shotcrete Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 506 Published: 8/2021 Regular Price: $ 79.00 USD Member Price: $ 79.00 USD Become a Member More Info »
ACI PRC-544.9-17: Report on Measuring Mechanical Properties of Hardened Fiber-Reinforced Concrete Topic: Fiber-Reinforced Concrete Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 544 Published: 1/2017 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-549.5-16 Report on Spray-up and Continuous Strand Glass Fiber Reinforced Concrete (GFRC) Topic: Fiber-Reinforced Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 549 Published: 2/2016 Price:$ 81.50 USD Become a Member More Info »
ACI PRC-544.10-21: Fiber Effect on Reducing the Permeability of Cracked Concrete Structures—TechNote Topic: Cracking , Durability , Fiber-Reinforced Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 544 Published: 6/2021 Price:$ 19.00 USD Become a Member More Info »