PRC-377-21: Integrity and Collapse Resistance of Structural Concrete Floor Systems - Report

Abstract:

This report provides a summary of the present understanding of collapse-resisting mechanisms of reinforced concrete and post-tensioned flat plates, flat slabs, slabs with beams, joist floor systems, and precast floor systems following initial local failures.