PRC-364.4-21: Determining the Load Capacity of a Structure when Structural Drawings are Unavailable - TechNote

Abstract:

When a structural evaluation to determine capacity is to be performed, knowledge of member sizes, reinforcing details, and material properties is required. In cases where this information is not readily available through drawing document records, it needs to be obtained through in-place measurements and sampling.