Alkali Aggregate Reaction

Definition: chemical reaction in either mortar or concrete between alkalies (sodium and potassium) from portland cement or other sources and certain constituents of some aggregates.- ACI Concrete Terminology


Alkali-aggregate reactions can be either alkali-carbonate reactions (ACRs) or alkali-silica reactions (ASRs). In ACR, the reaction is between the alkalies (sodium and potassium) and certain carbonate rocks, particularly calcitic dolomite and dolomitic limestones, present in some aggregates. In ASR, the reaction is between alkalies and certain siliceous rocks or minerals, such as opaline chert, strained quartz, and acidic volcanic glass, present in some aggregates.

Practice oriented papers and articles ON ALKALI AGGREGATE REACTION

Effect of Aggregate Types on Mortar Properties Produced with Geopolymer Binders

Publication: Special Publication
Date: 4/22/2021

Interactions Between SCM`S and Different Aggregates for Preventing ASR

Publication: Special Publication
Date: 4/22/2021

The Use of Ground Glass as a Pozzolan

Publication: Special Publication
Date: 4/22/2021

ASR-Related Distress in Floor Coatings

Publication: Concrete International
Date: 11/1/2019

Resistance of Hybrid Cement after 5 Years of Exposure to 5% Na2SO4

Publication: Special Publication
Date: 9/26/2018

Compressive Strength and Durability of Concrete Made with Combined Cementitious Materials

Publication: Special Publication
Date: 9/26/2018

Deterioration Survey of Structural Concrete at the Rogun Hydro after its Conservation

Publication: Special Publication
Date: 8/10/2018

Durability of Recycled Aggregate Concrete: A Review

Publication: Special Publication
Date: 3/1/2017

Alkali Silica Reaction in Mortar at Room Temperature

Publication: Special Publication
Date: 10/1/2016

Suppressing Alkali-Silica Expansion

Publication: Concrete International
Date: 5/1/2016

Search all Articles on Alkali Aggregate Reaction »


ACI Web Pages


Advanced Tips
Type Example Notes
Fuzzy kettle~ Contain terms that are close to the word kettle, such as cattle
Wild cat* Contain terms that begin with cat, such as category and the extact term cat itself
Exact-Single orange Contain the term orange
Exact-Phrase "dnn is awesome" Contain the exact phase dnn is awesome
OR orange bike Contain the term orange or bike, or both. OR, if used, must be in uppercase
orange OR bike
AND orange AND bike Contain both orange and bike. AND must be in uppercase
Combo (agile OR extreme) AND methodology Contain methodology and must also contain agile and/or extreme
Results Per Page:
select
Limit the search results with the specified tags
Limit the search results modified within the specified time
select
Limit the search results from the specified source
select
Search results must exactly contain the keywords

Please enter this 5 digit unlock code on the web page.