ACI PRC-132.2-22: Responsibility in Concrete Rehabilitation Construction - Guide Topic: Codes Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 132 Published: 3/2023 Regular Price: $ 89.00 USD Member Price: $ 59.00 USD Become a Member More Info »
ACI PRC-201.2-23: Durable Concrete—Guide Topic: Codes , Durability Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 201 Published: 5/2023 Price:$ 119.00 USD Become a Member More Info »
ACI PRC-207.1-21: Mass Concrete—Guide Topic: Codes Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 207 Published: 2/2022 Regular Price: $ 69.00 USD Member Price: $ 39.00 USD Become a Member More Info »
ACI PRC-207.2-07 Report on Thermal and Volume Change Effects on Cracking of Mass Concrete Topic: Codes , Mass Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 207 Published: 8/2007 Price:$ 61.50 USD Become a Member More Info »
ACI PRC-207.3-18: Report on Practices for Evaluation of Concrete in Existing Massive Structures for Service Conditions Topic: Codes , Mass Concrete Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 207 Published: 1/2018 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-207.5-11 Report on Roller-Compacted Mass Concrete Topic: Codes , Mass Concrete Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 207 Published: 7/2011 Price:$ 101.50 USD Become a Member More Info »
ACI PRC-207.6-17: Report on the Erosion of Concrete in Hydraulic Structures Topic: Codes Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 207 Published: 9/2017 Price:$ 54.50 USD Become a Member More Info »
ACI PRC-209.1-05: Report on Factors Affecting Shrinkage and Creep of Hardened Concrete Topic: Codes , Creep & Shrinkage Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 209 Published: 9/2005 Price:$ 40.50 USD Become a Member More Info »
ACI PRC-209.2-08 Guide for Modeling and Calculating Shrinkage and Creep in Hardened Concrete Topic: Codes , Creep & Shrinkage Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 209 Published: 4/2008 Price:$ 78.50 USD Become a Member More Info »
ACI PRC-211.1-22: Selecting Proportions for Normal-Density and High Density-Concrete - Guide Topic: Codes Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: ACI Committee 211 Published: 7/2022 Price:$ 99.00 USD Become a Member More Info »
ACI PRC-211.10-24: Assessing Combined Aggregate Gradings—Guide Topic: Codes Format: Printed Document or Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 211 Published: 12/2024 Price:$ 54.00 USD Become a Member More Info »
ACI PRC-211.4-08: Guide for Selecting Proportions for High-Strength Concrete Using Portland Cmt & Other Cementitious Material Topic: Codes , Mixture Proportioning Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 211 Published: 1/2009 Price:$ 60.50 USD Become a Member More Info »
ACI PRC-211.8-15 (Reapproved 2023) Guide to Troubleshooting Concrete Mixture Issues as Influenced by Constitutive Materials, Jobsite Conditions Topic: Codes , Mixture Proportioning Format: PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 211 Published: 7/2015 Price:$ 51.50 USD Become a Member More Info »
ACI PRC-212.3-16 Report on Chemical Admixtures for Concrete Topic: Admixtures , Codes Format: PDF or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 212 Published: 4/2016 Price:$ 99.50 USD Become a Member More Info »
ACI PRC-213-14(23) Guide for Structural Lightweight-Aggregate Concrete Reapproved 2023 Topic: Codes Format: Protected PDF/Web View, PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English or Spanish Author: ACI Committee 213 Published: 7/2014 Price:$ 95.50 USD Become a Member More Info »