Description
This specification describes the work of repairing defects in hardened portland cement concrete with a sand-filled mortar using an adhesive binder such as defined in ASTM C 881. It includes controls for adhesive labeling storage, handling, mixing and application, surface evaluation and preparation as well as inspection and quality control.
Keywords: bond (concrete to concrete); concrete construction; epoxy resins, hardened concrete; mortars (material); quality control; repairs; resurfacing; specifications; standards.
Document Details
Author: ACI Committee 503
ISBN: 9780870318757
Categories: Epoxies
Formats: PDF
This document is Historical
ERRATA INFO
Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the
Errata page.
Return/Exchange Policy
Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
Subscriptions These items are not eligible for return.
Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).