This report covers state-of-the-art of accelerated concrete paving techniques. Accelerated concrete paving techniques are appropriate for roadways, airfields, streets and intersections, and other paved surfaces where early opening to traffic and quick access are required. Considerations include planning, concrete materials and properties, jointing and joint sealing, curing and temperature control, concrete strength testing, and opening-to-traffic criteria. Applications and uses of accelerated concrete paving are discussed.

Keywords: accelerated paving; admixtures; aggregates; airports; concrete pavement; curing; fast-track paving; gradation; highways; intersections; joint sealing compound; jointing; specifications; streets.

 

Document Details

Author: ACI Committee 325

Pages: 24

ISBN: 9781641950558

Categories: Pavements

Formats: PDF

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1—Introduction

1.2—Scope

CHAPTER 2—NOTATION AND DEFINITIONS

2.1—Notation

2.2—Definitions

CHAPTER 3—PROJECT APPLICATIONS

3.1—Highways and tollways

3.2—Streets

3.3—Intersections

3.4—Airports

CHAPTER 4—PLANNING

4.1—Planning considerations

4.2—Partnering

4.3—Specifications

4.4—Innovative equipment

CHAPTER 5—CONCRETE MATERIALS

5.1—Concrete mixture proportioning

5.2—Cement

5.3—Supplementary cementitious materials

5.4—Air-entraining admixtures

5.5—Water-reducing admixtures

5.6—Accelerating admixtures

5.7—Aggregate

5.8—Water

CHAPTER 6—CONSTRUCTION

6.1—General

6.2—Other materials and methods

6.3—Finishing and texturing

6.4—Curing and temperature management

6.5—Jointing and sealing

CHAPTER 7—NONDESTRUCTIVE TESTING

7.1—Appropriate methods

7.2—Maturity

CHAPTER 8—TRAFFIC OPENING

8.1—Strength criteria

8.2—Construction traffic

8.3—Public traffic

8.4—Aircraft traffic

CHAPTER 9—REFERENCES

Authored documents

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).