305.1-14 Specification for Hot Weather Concreting

305.1-14 Specification for Hot Weather Concreting

Currency Choice

Your Price: $ 42.50 USD

Member Price: $ 26.00 USD

Save $ 16.50 USD, Become a Member

Choose Product Language

Choose Product Format

Notes/Preview

Preview

Description

This reference specification provides requirements for hot weather concreting that the architect/engineer can apply to any construction project involving hot weather concreting by citing it in the project specification. Checklists are provided to assist the architect/engineer in supplementing the provisions of this reference specification as needed by designating or specifying customized project requirements. This specification includes hot weather requirements for production preparations, delivery, placement, finishing, bleed-water evaporation, curing, and concrete protection. Provisions governing a preplacement conference, concrete mixture proportions, maximum allowable concrete temperature, rate of surface evaporation measurements, evaporation control measures, and acceptance of a concrete mixture from past field experience or preconstruction testing are also included.

Keywords: bleeding; curing; evaporation; finishing; mixture proportioning; plastic shrinkage cracking; protection period; trial batch.

 

Document Details

Author: ACI Committee 305

Publication Year: 2014

Pages: 7.00

ISBN: 9780870319167

Categories: Hot Weather

Formats: Printed Document, PDF, ePub, or Kindle

Table of Contents

Section 1- General

1.1—Scope

1.2––Definitions

1.3—Reference Standards

1.4—Submittals

1.5––Quality assurance, quality control, and acceptance of work

Section 2- Products

2.1—General

Section 3- Execution

3.1—General

3.2—Maximum temperature of fresh concrete at time of discharge

3.3—Qualification of concrete mixture

3.4—Concrete production and delivery

3.5—Concrete placement and finishing

3.6—Concrete bleed-water evaporation

3.7—Concrete curing

3.8—Concrete protection

Notes to Specifier

General notes

Foreword to checklists

Appendix A

Example of Uno Equation used to determine surface evaporation rate of fresh concrete.

Appendix B

Example of NRMCA nomograph for estimating surface evaporation rate on the basis of menzel formula

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).