Q. What is an air-entraining admixture? A. It is an admixture that causes the development of a system of microscopic air bubbles in cement paste during mixing, usually to increase its resistance to freezing and thawing and to improve workability (ACI 212.3R). References: SP-1(02); CCS-0(16); ACI CT-23; E4-22; ACI 212.3R-16; SP-288; ACI 306R-16; ASTM C260; ASTM C494 Topics in Concrete: Admixture; Concrete Fundamentals; Materials; Cold Weather
Q. What is an air-entraining admixture?
A. It is an admixture that causes the development of a system of microscopic air bubbles in cement paste during mixing, usually to increase its resistance to freezing and thawing and to improve workability (ACI 212.3R).
References: SP-1(02); CCS-0(16); ACI CT-23; E4-22; ACI 212.3R-16; SP-288; ACI 306R-16; ASTM C260; ASTM C494
Topics in Concrete: Admixture; Concrete Fundamentals; Materials; Cold Weather