Concrete Strength Testing Technician

ACI Certification Sessions Calendar

ACI sponsoring groups are continually adding new instruction and testing sessions. Many upcoming sessions are listed below; however, you should contact the ACI testing center(s) in your area for a complete listing of sessions and/or to schedule an exam or training session. Find a testing center

ACI RESOURCE CENTERS

The ACI Resource Center coordinates with ACI chapters and sponsoring groups to offer direct, on-demand access to all ACI Certification programs, plus hands-on training and educational opportunities.

Southern California »

Chicago/Midwest »

Mid-Atlantic »

4 easy steps to get aci certified

Learn how to get certified through ACI.

learn more »

Questions?

Contact the ACI Certification Department+1.248.848.3790

 
Concrete Strength Testing Technician

February 26, 2026 to February 26, 2026
Starting Time:   1:00pm CST
End Time:   5:00pm CST

University of New Orleans
Lakefront Campus
New Orleans , LA   United States
Sponsor(s): MAC Engineering

Description:
Exam Session Date & Time
February 26, 2026 – 1:00pm CST

Exam Location
University of New Orleans
Lakefront Campus
Engineering Building Room 119

Program Information
Exam Scope

C 617 Capping Cylindrical Concrete Specimens
C 39 Compressive Strength of Cylindrical Concrete Specimens
C 1231 Unbonded Caps for Concrete Cylinders
C 78 Flexural Strength of Concrete


The one-hour written examination is closed book and consists of approximately 40 multiple-choice questions. The required passing grade for the written examination is at least 60% correct for each of the required standards and a minimum score of 70% overall.

Study Material
Technician Workbook for ACI Strength Testing Technician, ACI CP-19 (25th edition)
Order with registration or order directly from ACI online at www.concrete.org

General Information
For additional information contact Mark A. Cheek at mark@macheek.us.
Program size will be limited to a minimum of 5 and a maximum of 10. Cancellation Policy: you must cancel 5 days prior to exam to receive a 100% refund thereafter the full fee will be forfeited.
For additional on-line info, click on the link below:
http://www.acilouisiana.org

For more information, contact:
Mark A Cheek, P.E., FACI
MAC Engineering
Mandeville, LA    70448-2236    United States
Email: mark@macheek.us
Phone: (504) 343-7151