Read and study the material for this module. Then, complete and pass the corresponding 10-question quiz with a score of 80% or higher to receive a certificate for 0.1 CEU (equivalent to 1.0 PDH). This online course is not approved for credit with the Florida Construction Industry Licensing Board (CILB). 
Continuing Education Credit: 0.1 CEU (1 PDH)
Access Period: 180 days
This course is included in the Anchorage Design Certificate Program. Completion of all courses in an ACI University Certificate Program will earn you a program certificate and digital badge. For more details, visit ACI University Certificate Programs.
                    
                    
                        
                            Description 
                            This module covers Chapter 7 of ACI 355.4-11, “Qualification of Post-Installed Adhesive Anchors in Concrete (ACI 355.4-11).”  This document prescribes testing programs and evaluation requirements for post-installed adhesive anchors intended for use in concrete under the design provisions of ACI 318. This chapter covers the reliability testing requirements including sensitivity to hole cleaning (dry, saturated, and submerged concrete),mixing effort, moisture (dry, saturated, and submerged concrete), crack width (in low-strength and high-strength concrete), freezing and thawing, and sustained loading.
This document is covered in three parts.
                        
                    
                
                
                        Table of Contents 
                        Learning Objectives:
1. Recognize the purpose of reliability testing to establish the anchor system is capable of safe, effective behavior under normal and adverse installation conditions;
2. Identify the procedures for the sensitivity testing of anchor systems for various conditions including freezing and thawing, mixing effort, hole cleaning, moisture, crack width, and sustained loading;
3. Understand the labeling for products not tested for sensitivity to installation orientation; and
4. Know that the reliability tests are not accountable for addressing gross installation errors such as deviations from the specified embedment depth, and use of a nominal diameter drill bit other than that specified.
                    
                
                
                    
                        Return/Exchange Policy 
                        Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.
                        Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.
                        Subscriptions These items are not eligible for return.
                        Exchanges:  Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).