Definition: a composite structural material comprising thin sections consisting of cement mortar reinforced by a number of closely spaced layers of steel wire mesh.- ACI Concrete Terminology
View all Documents on Ferrocement »
Publication: IJCSM Date: 9/30/2025
Publication: IJCSM Date: 9/30/2024
Publication: IJCSM Date: 1/31/2024
Publication: IJCSM Date: 7/31/2023
Publication: Materials Journal Date: 11/1/2019
Publication: Structural Journal Date: 3/1/2017
Publication: Structural Journal Date: 11/1/2015
Publication: Materials Journal Date: 3/1/2008
Publication: Materials Journal Date: 2/1/2008
Search all Articles on Ferrocement »
Publication: Special Publication Date: 10/1/2023
Publication: Concrete International Date: 11/1/2012
Publication: Concrete International Date: 3/1/2012
Publication: Special Publication Date: 10/1/2010
Publication: Special Publication Date: 12/1/2004
Publication: Special Publication Date: 4/1/2002
Publication: Special Publication Date: 6/1/2001
Publication: Concrete International Date: 10/1/2000
Publication: Special Publication Date: 8/1/2000
There are no Certification Resources on Ferrocement
View all ACI Certification Resources on Ferrocement »
There are no Education Publications on Ferrocement
View all ACI Education Publications on Ferrocement »
There are no Online Learning Courses on Ferrocement
View all ACI Online Learning Courses on Ferrocement »
by Fantilli
View all free presentations on Ferrocement »
There are no faqs on Ferrocement
View all Frequently Asked Questions »
There are no Events on Ferrocement
View all Ferrocement Events »
April 9, 2026
Scott Anderson elected President of the American Concrete Institute
March 23, 2026
ACI's New Honorary Members – 2026
June 12, 2025
ACI congratulates Dr. Antonio Nanni on AAU research productivity recognition
May 1, 2023
Unparalleled Opportunities at ACI
April 27, 2023
Antonio Nanni Elected President of American Concrete Institute
April 2, 2021
Cary S. Kopczynski Elected President of American Concrete Institute
March 3, 2021
ACI’s New Honorary Members
May 26, 2020
ACI India Chapter Conducts its 2020 Excellence in Concrete Construction Awards
July 18, 2019
ACI Iraq Chapter Announces Winners of the 2019 Student Project Competition
October 23, 2018
American Concrete Institute Announces Winners of Pervious Concrete Cylinder Student Competition
View All ACI News »
Thin Reinforced Cementitious Products and Ferrocement
Search all Committees »
There are no Certifications on Ferrocement
View all certification programs »