ACI PRC-334.1-22: Concrete Shell Structures - Guide Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units Language: English Author: Joint ACI-ASCE Committee 334 Published: 6/2022 Regular Price: $ 54.00 USD Member Price: $ 34.00 USD Become a Member More Info »
ACI PRC-334.3-05(20): Construction of Concrete Shells Using Inflated Forms Topic: Shells Format: Protected PDF/Web View Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 334 Published: 10/2005 Price:$ 74.50 USD Become a Member More Info »
ACI PRC-334.1-92: Concrete Shell Structures Practice and Commentary (Reapproved 2002) Topic: Shells Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 334 Published: 8/2002 Price:$ 31.50 USD Become a Member More Info »