ACI PRC-121-08 Guide for Concrete Construction Quality Systems in Conformance with ISO 9001 Topic: Admixtures Format: PDF Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 121 Published: 7/2008 Price:$ 67.50 USD Become a Member More Info »
ACI PRC-121.1-16: Guide to Quality Management Auditing in the Concrete Industry Topic: Quality Assurance Format: Printed Document, PDF, ePub, or Kindle Unit: IN-LB: Inch-Pound Units and SI: International System of Units Language: English Author: ACI Committee 121 Published: 1/2017 Price:$ 54.50 USD Become a Member More Info »