Table of Contents
506-16: GUIDE TO SHOTCRETE
PREFACE
Introduction
History
Applications
New developments
Research and development
CHAPTER 1—INTRODUCTION AND SCOPE, p. 2
1.1—Introduction, p. 2
1.2—Scope, p. 3
CHAPTER 2—DEFINITIONS, p. 3
CHAPTER 3—INSULATING CONCRETE FORM SYSTEMS, p. 3
3.1—Flat-wall, p. 3
3.2—Additional ICF systems, p. 3
CHAPTER 4—MATERIALS, p. 5
4.1—Concrete mixture, p. 5
4.2—Reinforcing materials overview, p. 6
CHAPTER 5—INSULATING CONCRETE FORMS, p. 6
5.1—Formwork material, p. 6
5.2—Formwork configurations, p. 6
5.3—Insulating concrete form components, p. 7
5.4—Material performance requirements, p. 8
5.5—Bracing and scaffolding, p. 9
5.6—Miscellaneous, p. 9
CHAPTER 6—DESIGN AND ACI 318 APPLICATION, p. 9
6.1—General, p. 9
6.2—Flat wall ICF systems: application of ACI 318, p. 10
6.3—Waffle grid ICF wall systems: application of ACI 318, p. 11
6.4—Screen grid and post-and-beam ICF wall systems: application of ACI 318, p. 12
6.5—Other design resources for ICF wall systems, p. 13
CHAPTER 7—CONSTRUCTION, p. 13
7.1—Planning the construction process, p. 13
7.2—Foundation/multiple level considerations, p. 14
7.3—Reinforcing steel placement considerations, p. 14
7.4—Work implementation, p. 14
CHAPTER 8—REFERENCES, p. 15
Authored documents, p. 16
Appendix A: Design Examples (inch-pound units), p. 17
A.1—Engineered design examples, p. 17
Appendix B: Design Examples (SI units), p. 32
B.1—Engineered design examples, p. 32
APPENDIX REFERENCES, p. 49
506.2-13: SPECIFICATION FOR SHOTCRETE (REAPPROVED 2018)
PART 1—GENERAL
1.1—SCOPE
1.2—DEFINITIONS
1.3—REFERENCED STANDARDS
1.4—SUBMITTALS
1.5—PRECONSTRUCTION TESTING BY CONTRACTOR
1.6—TESTING DURING CONSTRUCTION
1.7—DELIVERY, STORAGE, AND HANDLING
PART 2—PRODUCTS
2.1—MATERIALS
2.2—PACKAGED SHOTCRETE MATERIALS
2.3—FIBER-REINFORCED SHOTCRETE
2.4—SHOTCRETE PROPERTIES
2.5—PROPORTIONING
2.6—BATCHING, MIXING, AND DELIVERY
PART 3—EXECUTION
3.1—PREPARATION OF SURFACE TO RECEIVE SHOTCRETE
3.2—JOINTS
3.3—ALIGNMENT CONTROL
3.4—APPLICATION
3.5—FINISH
3.6—CURING
3.7—PROTECTION
3.8—TOLERANCES
3.9—REPAIR OF SHOTCRETE
3.10—ACCEPTANCE OF WOR
(NONMANDATORY PORTION FOLLOWS)
NOTES TO SPECIFIER
GENERAL NOTES
FOREWORD TO CHECKLISTS
CHECKLIST REFERENCES
(MANDATORY PORTION FOLLOWS)