Description

This guide provides practical information about the construction of quality residential concrete. It covers concrete work for one- and two-family dwellings with a maximum height of two stories above grade and a basement that is either cast-in-place or placed as precast elements. Information on materials ,proportions, production, delivery, and testing is provided. Separate chapters on footings, walls, and slabs provide information on subgrade, forms, reinforcement, placement, consolidation, finishing, and curing. Special considerations regarding insulation and hot and cold weather are included. Common problems and their repair are also addressed. The discussion ofspecific design provisions and all drawings provided by this guide are intended to offer illustrations of typical practice and should not be interpreted as meeting the requirements of specific codes or project specifications. Applicable codes and construction documents take precedence over the information contained in this document.

Keywords: finish; footing; form; slab; slab-on-ground; subgrade; tolerance;wall.

 

Document Details

Author: ACI Committee 332

Publication Year: 2006

Pages: 48

ISBN: 9780870312267

Categories: Residential

Formats: PDF

This document is Historical

Table of Contents

Chapter 1—Introduction

1.1—Scope

1.2—Definitions

Chapter 2—Concrete

2.1—Fundamentals

2.2—Materials

2.3—Mixture proportioning

2.4—Ordering

2.5—Production and delivery

2.6—Testing

Chapter 3—Footings

3.1—Purpose

3.2— Excavation

3.3— Soil

3.4— Footing types

3.5— Footing loads

3.6—Tolerances

3.7—Form types

3.8—Geometry

3.9—Concrete

3.10—Reinforcement

3.11—Placement

3.12—Curing and protection

3.13—Footing drainage

Chapter 4—Walls

4.1—Forming systems

4.2—Precast systems

4.3—Reinforcement

4.4—Geometry

4.5—Wall construction

4.6—Curing and protection

4.7—Moisture protection

4.8—Backfilling

4.9—Safety

Chapter 5—Slabs

5.1—Slabs-on-ground

5.2—Elevated slabs

5.3—Concrete

5.4—Placing and finishing

5.5—Jointing

5.6—Curing

Chapter 6—Project considerations

6.1—Ordering ready-mixed concrete

6.2—Site considerations

6.3—Placement considerations

6.4—Special materials

6.5—Hot weather concreting

6.6—Cold weather concreting

6.7—Troubleshooting

Chapter 7—References

7.1—Referenced standards and reports

7.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).