309.2R-98: Identification and Control of Visible Effects of Consolidation on Formed Concrete Surfaces (Reapproved 2005)

309.2R-98: Identification and Control of Visible Effects of Consolidation on Formed Concrete Surfaces (Reapproved 2005)

Currency Display

Your Price:$ 26.00 USD

Member Price: $ 16.00 USD

Save $ 10.00 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**A newer version of this document exists**

NEW VERSION

 

Description

This report provides guidelines for identifying and controlling visible effects of consolidation on precast or cast-in-place formed concrete surfaces. It includes a summary of direct and indirect causes of such imperfections. An outline to assist in the reporting on surfaces and photographs to illustrate typical concrete blemishes are also included.

 

Document Details

Author: ACI Committee 309

Publication Year: 2017

Pages: 11

ISBN: 9780870310188

Categories: Consolidation

Formats: PDF

This document is Historical

Table of Contents

Chapter 1--General

Chapter 2--Factors causing effects

2.1--Design of structural members

2.2--Specifications

2.3--Forms

2.4--Properties of fresh concrete

2.5--Placement

2.6--Consolidation

2.7--Special construction conditions

Chapter 3--Surface defects

3.1--Honeycomb

3.2--Air surface voids

3.3--Form-streaking

3.4--Aggregate transparency

3.5--Subsidence cracking

3.6--Color variation

3.7--Sand streaking

3.8--Layer lines

3.9--Form offsets

3.10--Cold joints

Chapter 4--Minimizing surface defects

Chapter 5--Consolidation of preplaced aggregate concrete

Chapter 6--Conclusion

Chapter 7--References

7.1--Recommended references

7.2--Cited references

Chapter 8--Surface condition outline

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).