Guidance is provided on the use of methods to estimate the in-place strength of concrete in new and existing construction. The methods include: rebound number, penetration resistance, pullout, break-off, ultrasonic pulse velocity, maturity, and cast-in-place cylinders. The principle, inherent limi­tations, and repeatability of each method are reviewed. Procedures are presented for developing the relationship needed to estimate compressive strength from in-place results. Factors to consider in planning in-place tests are discussed, and statistical techniques to interpret test results are presented. The use of in-place tests for acceptance of concrete is intro­duced. The appendix provides information on the number of strength levels that should be used to develop the strength relationship and explains a regression analysis procedure that accounts for error in both dependent and independent variables.

Keywords: coefficient of variation; compressive strength; construction; in-place tests; nondestructive tests; safety; sampling; statistical analysis.

 

Document Details

Author: ACI Committee 228

Publication Year: 2003

Pages: 44

ISBN: 9780870311321

Categories: Nondestructive Evaluation

Formats: PDF

This document is Historical

Table of Contents

Chapter 1—Introduction

1.1—Scope

1.2—Need for in-place tests during construction

1.3—Influence of ACI 318

1.4—Recommendations in other ACI documents

1.5—Existing construction

1.6—Objective of report

Chapter 2—Review of methods

2.1—Introduction

2.2—Rebound number (ASTM C 805)

2.3—Penetration resistance (ASTM C 803/C 803M)

2.4—Pullout test (ASTM C 900)

2.5—Break-off number (ASTM C 1150)

2.6—Ultrasonic pulse velocity (ASTM C 597)

2.7—Maturity method (ASTM C 1074)

2.8—Cast-in-place cylinders (ASTM C 873)

2.9—Strength limitations

2.10—Combined methods

2.11—Summary

Chapter 3—Statistical characteristics of test results

3.1—Need for statistical analysis

3.2—Repeatability of test results

Chapter 4—Development of strength relationship

4.1—General

4.2—New construction

4.3—Existing construction

Chapter 5—Implementation of in-place testing

5.1—New construction

5.2—Existing construction

Chapter 6—Interpretation and reporting of results

6.1—General

6.2—Statistical methods

6.3—Reporting results

Chapter 7—In-place tests for acceptance of concrete

7.1—General

7.2—Acceptance criteria

7.3—Early-age testing

Chapter 8—References

8.1—Referenced standards and reports

8.2—Cited references

Appendix

A.1— Minimum number of strength levels

A.2—Regression analysis with X-error (Mandel 1984)

A.3—Standard deviation of estimated Y-value (Stone and Reeve 1986)

A.4—Example

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).