Description

This guide is intended for use in establishing basic duties and reports required of inspection personnel. It can be used for all types and sizes of projects but should be supplemented with additional inspection requirements when the complexity of the project so dictates. Refer to ACI 311.4R for guidance on additional requirements and to SP-2 for more detailed information on concrete production practices and inspection and testing of concrete.

This guide recommends minimum requirements for inspection at the concrete plant when such inspections are required by specifications or the owner. It also recommends minimum requirements for field and laboratory testing of concrete. It is intended for use by specifiers, architects, engineers, owners, contractors, or other groups needing to monitor the ready-mixed concrete producers’ activities at the concrete plant and concreting activities at the project site through the use of an independent inspection agency or in-house inspection organization.

This guide also recommends minimum testing laboratory qualifications, minimum inspector qualifications, duties, and reports.

Keywords: batch plants; contract documents; curing; high-strength concrete;

quality control; ready-mixed concrete; test.

 

Document Details

Author: ACI Committee 311

Publication Year: 2004

Pages: 6

ISBN: 9780870311482

Categories: Inspection

Formats: PDF

This document is Withdrawn

Table of Contents

Chapter 1—Plant inspection of ready-mixed concrete

1.1—Introduction and scope

1.2—Inspector qualifications

1.3—Inspector duties

1.4—Reports

Chapter 2—Testing of ready-mixed concrete

2.1—Introduction and scope

2.2—Qualifications

2.3—Testing laboratory

2.4—Duties

2.5—Testing high-strength concrete

2.6—Reports

Chapter 3—References

3.1—Referenced standards and reports

3.2—Other references

3.3—Laboratory evaluation and accreditation agencies

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).