A complex problem analyzed and defined. Seven papers presented at the Symposium on Concrete Shell Buckling. Organizes in one handy volume up- todate information on buckling.

Subject matter includes: overview of buckling of reinforced concrete shells compared to general stability and the stability of concrete columns and plates; design of several shell types-cylindrical, domicai, hyperbolic, and elliptic paraboloids, folded plates, and hyperbolic cooling towers; analytical techniques for investigating shell buckling; and experimental techniques for investigating buckling in light of practical applications.

 

Document Details

Publication Year: 1981

ISBN: 9780870317392

Categories: Shells

Formats: PDF

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).