This report outlines existing procedures for testing and measuring fresh state performance and fiber dispersion in fiber-reinforced concrete (FRC). As for the former, test methods applicable to both ordinary vibrated FRC and fiber-reinforced self-consolidating concrete (FR-SCC) are reviewed. Methods for nondestructive monitoring of fiber dispersion and orientation in FRC materials and structures are also presented and their pros and cons addressed.

Keywords: fiber dispersion; fiber-reinforced concrete; fresh state performance; nondestructuive testing; self-consolidating fiber-reinforced concrete.

 

Document Details

Author: ACI Committee 544

Publication Year: 2017

ISBN: 9781945487644

Categories: Codes, Fiber-Reinforced Concrete

Formats: PDF, ePub, or Kindle

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE

1.1—Introduction

1.2—Scope

CHAPTER 2—NOTATION AND DEFINITIONS

2.1—Notation

2.2—Definitions

CHAPTER 3—FRESH STATE PROPERTIES

3.1—Sampling, unit weight, yield, and air content

3.2—Workability and fresh state performance

3.3—Rheometer tests

CHAPTER 4—FIBER DISPERSION AND ORIENTATION

4.1—General

4.2—Destructive method

4.3—Nondestructive methods

CHAPTER 5—CONCLUSION AND SUMMARY OF TEST METHODS

CHAPTER 6—REFERENCES

Authored documents

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).