ACI PRC-544.11-22: Measuring Shrinkage, Creep, and Transport Properties of Fiber-Reinforced Concrete—Report

ACI PRC-544.11-22: Measuring Shrinkage, Creep, and Transport Properties of Fiber-Reinforced Concrete—Report

Currency Display

Your Price:$ 54.00 USD

Member Price: $ 34.00 USD

Save $ 20.00 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Description

Fiber-reinforced concrete (FRC) has become a viable choice for many designers and builders for the unique properties and advantages it provides. From slabs-on-ground to underground structures, the use of FRC has been expanding in concrete construction. This growth of applications has created the need to review the existing test methods for FRC and, where necessary, develop new ones. Two reports (ACI 544.2R and ACI 544.9R) have already been published regarding testing fresh properties and mechanical properties of FRC, respectively. This report is the third and final report on testing FRC for its durability properties, including shrinkage, creep, and permeability. Several standard and nonstandard test methods are presented in this report to represent some of the knowledge in this area.

Keywords:

creep; durability; fiber-reinforced concrete; shrinkage; testing; transporting.

 

Document Details

Author: ACI Committee 544

Publication Year: 2022

Pages: 19

ISBN: 9781641951814

Categories: Codes

Formats: Protected PDF/Web View

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE, p. 2

1.1—Introduction, p. 2

1.2—Scope, p. 3

CHAPTER 2—DEFINITIONS, p. 3

CHAPTER 3—TESTING SHRINKAGE OF FRC, p. 3

3.1—Shrinkage in concrete and FRC, p. 3

3.2—Testing FRC for free (unrestrained) shrinkage, p. 4

3.3—Testing FRC for restrained shrinkage, p. 5

CHAPTER 4—TESTING CREEP PROPERTIES OF FRC, p. 8

4.1—Creep behavior of concrete and FRC, p. 8

4.2—Testing FRC for creep, p. 8

CHAPTER 5—TESTING DURABILITY PROPERTIES OF FRC, p. 12

5.1—Transport properties in concrete and FRC, p. 12

5.2—Testing FRC for chloride diffusion, p. 12

5.3—Testing FRC for water permeability, p. 14

CHAPTER 6—CONCLUSIONS, p. 16

CHAPTER 7—REFERENCES, p. 17

Authored documents, p. 17

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).