ACI SPEC-503.3-10 Specification for Producing a Skid-Resistant Surface on Concrete by the Use of Epoxy and Aggregate

ACI SPEC-503.3-10 Specification for Producing a Skid-Resistant Surface on Concrete by the Use of Epoxy and Aggregate

Currency Display

Your Price:$ 39.50 USD

Member Price: $ 26.00 USD

Save $ 13.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**A newer version of this document exists**

NEW VERSION

 

Description

This specification describes the work of producing a skid-resistant surface on hardened concrete by the application of a multi-component epoxy resin. It includes controls for resin labeling, storage, handling, mixing, and application; surface evaluation and preparation; and inspection and quality. In addition, it describes an aggregate to be used with the coating.

Keywords: aggregates; coatings; concrete pavements; epoxy resins; hardened concrete; quality control; skid resistance; specification; standards.

 

Document Details

Author: ACI Committee 503

Pages: 5

Categories: Codes, Polymer Concrete, Specifications

Formats: PDF

This document is Historical

Table of Contents

Part 1—General

1.1—Scope

1.2—Units of measurement

1.3—Reference standards

1.4—Definitions

1.5—Submittals

1.6—Quality assurance

1.7—Product delivery, storage, and handling

1.8—Project conditions

Part 2—Materials

2.1—General

2.2—Products

Part 3—Execution

3.1—Preparation of surfaces

3.2—Evaluate surface before coating application

3.3—Coating mixtures

3.4—Coating application

3.5—Field quality control

3.6—Cleanup

Notes to Specifier

General notes

(nonmandatory portion follows)

Foreword to checklists

Mandatory Requirements Checklist

Optional Requirements Checklist

Submittals Checklist

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).