Description

High-strength concrete (HSC) has emerged as a viable material to use as an alternative to conventional normal-strength concrete in infrastructure systems to reduce member cross section, extend member span length, reduce the number of system members, or enhance system sustainability. This guide offers general information on the quality control and testing of HSC. Recommendations are based on the current state of knowledge gained from worldwide experimental research, analytical work, and field applications of HSC systems used in concrete structures.

Keywords: acceptance criteria; compressive strength; concrete placement; creep; curing; delivery; modulus of elasticity; sampling; shrinkage; statistical concepts; strength evaluation; testing; trial batching; quality assurance; quality control.

 

Document Details

Author: ACI Committee 363

Publication Year: 2011

Pages: 19

ISBN: 9780870317033

Categories: High Performance Concrete

Formats: Protected PDF/Web View

Table of Contents

Chapter 1—Introduction and scope

1.1—Introduction

1.2—Scope

Chapter 2—Notation and definitions

2.1—Notation

2.2—Definitions

Chapter 3—Planning

3.1—Introduction

3.2—Preconstruction meeting

3.3—Trial batches

3.4—Prequalification of concrete suppliers and preconstruction testing

Chapter 4—Quality assurance and quality control

4.1—Introduction

4.2—Concrete plant

4.3—Delivery

4.4—Placing

4.5—Curing

Chapter 5—Testing

5.1—Introduction

5.2—Background

5.3—Sampling

5.4—Frequency of testing

5.5—Compressive strength specimens

5.6—Modulus of elasticity

5.7—Shrinkage and creep

5.8—Prequalification of testing laboratories

Chapter 6—Evaluation of compressive strength test results

6.1—Statistical concepts

6.2—Strength evaluation

Chapter 7—References

7.1—Referenced standards and reports

7.2—Cited references

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).