ACI SPEC-350.5-12 Specifications for Environmental Concrete Structures

ACI SPEC-350.5-12 Specifications for Environmental Concrete Structures

Currency Display

Your Price:$ 94.50 USD

Member Price: $ 59.00 USD

Save $ 35.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Notes/Preview


Preview

Description

This specification is a Reference Specification that the Architect/Engineer can make applicable to a construction project by citing it in the Project Specifications. The Architect/Engineer supplements the provisions of this Reference Specification as needed by designating or specifying individual project requirements. The document covers materials and proportioning of concrete; reinforcement and prestressing reinforcement; production, placing, finishing, and curing of concrete; formwork design and construction; and shotcrete. Methods of treatment of joints and embedded items, repair of surface defects, and finishing of formed and unformed surfaces are specified. Separate sections are devoted to architectural concrete, mass concrete, and internal and external post-tensioned prestressed concrete. Provisions governing testing, evaluation, and acceptance of concrete as well as acceptance of the structure are included.

Keywords: admixtures; aggregates; air entrainment; architectural concrete; compressive strength; consolidation; curing; density; durability; evaluation; environmental concrete; finishes; floors; formwork (construction); grouting; inspection; joints; mass concrete; mixture proportioning; posttensioned prestressed concrete; prestressing reinforcement; reinforcing steels; reshoring; shoring; subgrades; tolerances.

 

Document Details

Author: ACI Committee 350

Pages: 55

Categories: Codes, Environmental, Specifications

Formats: Protected PDF/Web View, ePub, or Kindle

Table of Contents

Section 1—General requirements

1.1—Scope

1.1.1—Work specified

1.1.2—Work not specified

1.2—Definitions

1.3—Reference standards

1.4—Standards-producing organizations

1.5—Submittals

1.5.1—General

1.5.2—Testing agency reports

1.6—Quality assurance

1.6.1—General

1.6.2—Testing agencies

1.6.3—Testing responsibilities of Contractor

1.6.4—Testing responsibilities of Owner’s Testing Agency

1.6.5—Tests on hardened concrete in-place

1.6.6—Evaluation of concrete strength tests

1.6.7—Acceptance of concrete strength

1.6.8—Field acceptance of concrete

1.7—Acceptance of structure

1.7.1—General

1.7.2—Dimensional tolerances

1.7.3—Appearance

1.7.4—Strength of structure

1.7.5—Durability

1.8—Protection of in-place concrete

1.8.1—Loading and support of concrete

1.8.2—Protection from mechanical injury

Section 2—Formwork and formwork accessories

2.1—General

2.1.1—Description

2.1.2—Submittals

2.2—Products

2.2.1—Materials

2.2.2—Performance and design requirements

2.2.3—Fabrication and manufacture

2.3—Execution

2.3.1—Construction and erection of formwork

2.3.2—Removal of formwork

2.3.3—Reshoring and backshoring

2.3.4—Strength of concrete required for removal of formwork

2.3.5—Field quality control

Section 3—Reinforcement and reinforcement supports

3.1—General

3.1.1—Submittals, data, and drawings

3.1.2—Materials delivery, storage, and handling

3.2—Products

3.2.1—Materials

3.2.2—Fabrication

3.3—Execution

3.3.1—Preparation

3.3.2—Placement

Section 4—Joints and accessories

4.1—General

4.1.1—Description

4.1.2—Submittals

4.2—Products

4.2.1—Materials

4.2.2—Performance and design requirements

4.3—Execution

4.3.1—General

4.3.2—Construction joints and other bonded joints

4.3.3—Contraction joints

4.3.4—Expansion joints

4.3.5—Waterstops

4.3.6—Smooth dowels

Section 5—Concrete mixtures

5.1—General

5.1.1—Description

5.1.2—Submittals

5.1.3—Quality control

5.1.4—Materials storage and handling

5.2—Products

5.2.1—Materials

5.2.2—Performance and design requirements

5.2.3—Proportioning

5.3—Execution

5.3.1—Measuring, batching, and mixing

5.3.2—Delivery

Section 6—Handling, placing, and constructing

6.1—General

6.1.1—Description

6.1.2—Submittals

6.1.3—Delivery, storage, and handling

6.2—Products

6.2.1—Materials

6.3—Execution

6.3.1—Preparation

6.3.2—Placement of concrete

6.3.3—Finishing formed surfaces

6.3.4—Finishing unformed surfaces

6.3.5—Curing and protection

6.3.6—Repair of surface defects

Section 7—Architectural concrete

7.1—General

7.1.1—Description

7.1.2—Submittals

7.1.3—Quality assurance

7.1.4—Product delivery, storage, and handling

7.1.5—Project conditions

7.2—Products

7.2.1—Materials

7.2.2—Performance and design requirements

7.3—Execution

7.3.1—Preparation

7.3.2—Proportioning concrete mixtures

7.3.3—Consolidation

7.3.4—Formwork monitoring

7.3.5—Formwork removal

7.3.6—Repair of tie holes and surface defects

7.3.7—Finishing

Section 8—Mass concrete

8.1—General

8.1.1—Description

8.1.2—Submittals

8.2—Products

8.2.1—Materials

8.2.2—Performance and design requirements

8.3—Execution

8.3.1—Placement

8.3.2—Curing and protection

Section 9—Internal post-tensioned concrete

9.1—General

9.1.1—Description

9.1.2—Submittals

9.1.3—Quality control

9.1.4—Product handling and storage

9.2—Products

9.2.1—Materials

9.2.2—Proportioning of cementitious grout mixtures

9.2.3—Proportioning of epoxy grout mixtures

9.3—Execution

9.3.1—Field observations

9.3.2—Grouted tendon installation

9.3.3—Grouting

9.3.4—Unbonded tendon installation

9.3.5—Tendon tolerances

9.3.6—Concrete placement

9.3.7—Tensioning

9.3.8—Tendon finishing

Section 10—External prestressed wrapped concrete tanks

10.1—General

10.1.1—Description

10.1.2—Submittals

10.1.3—Quality control

10.1.4—Product delivery, handling, and storage

10.2—Products

10.2.1—Materials

10.2.2—Proportioning of concrete and shotcrete mixtures

10.3—Execution

10.3.1—Placement

Notes to Specifier

General notes

Foreword to Checklists

Mandatory Requirements Checklist

Optional Requirements Checklist

Submittals Checklist

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).