ACI PRC-327.1-21: In-Place Density Testing of Freshly Placed Roller-Compacted Concrete by Nuclear Gauge Testing - TechNote

ACI PRC-327.1-21: In-Place Density Testing of Freshly Placed Roller-Compacted Concrete by Nuclear Gauge Testing - TechNote

Price: $ 19.00 USD

Choose Product Language

Choose Product Units


Choose Product Format


Description

What is the proper procedure for determining the in-place density of fresh roller-compacted concrete (RCC) according to ASTM C1040/C1040M, “Standard Test Methods for In-Place Density of Unhardened and Hardened Concrete, Including Roller Compacted Concrete, By Nuclear Methods?”

Keywords:

acceptance testing; backscatter; concrete density; direct transmission; in-place density; nuclear gauge; roller-compacted concrete (RCC).

 

Document Details

Author: ACI Committee 327

Publication Year: 2021

Pages: 4

ISBN:

Categories: Codes

Formats: Protected PDF/Web View

Table of Contents

Question

Answer

Discussion

Summary

References

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).