This Code provides material, design, and detailing requirements for cast-in-place and precast reinforced concrete chimneys. It sets forth minimum loadings for design and contains methods for determining the concrete and reinforcement required to obtain the strength required by the loadings. The methods of analysis apply primarily to circular chimney walls, but guidance is included for applying the general principles to noncircular chimney walls.

Keywords:

across-wind load; construction requirements; earthquake load; flexural strength; load combinations; reinforced concrete; reinforced concrete chimneys; structural design; thermal load; vortex shedding; windload.

 

Document Details

Author: ACI Commitee 307

Publication Year: 2023

Pages: 79

Categories: Codes

Formats: Printed Document or Protected PDF/Web View

Table of Contents

PREFACE, p. 3

CHAPTER 1—GENERAL, p. 4

1.1—Scope , p. 4

1.2—General, p. 4

1.3—Purpose, p. 4

1.4—Applicability, p. 5

1.5—Interpretation, p. 5

1.6—Building official, p. 6

1.7—Licensed design professional, p. 6

1.8—Construction documents and design records, p. 7

1.9—Testing and inspection, p. 7

CHAPTER 2—NOTATION AND DEFINITIONS, p. 8

2.1—Notation, p. 8

2.2—Definitions, p. 13

CHAPTER 3—REFERENCED STANDARDS, p. 14

CHAPTER 4—STRUCTURAL SYSTEM REQUIREMENTS, p. 15

4.1—Materials, p. 15

4.2—Design loads, p. 15

4.3—Structural system, p. 15

CHAPTER 5—CONCRETE: MATERIALS, DESIGN, AND DURABILITY REQUIREMENTS, p. 16

5.1—General, p. 16

5.2—Materials, p. 16

5.3—Concrete properties for design, p. 17

5.4—Durability requirements, p. 18

CHAPTER 6—REINFORCING STEEL: MATERIALS, DESIGN, AND DURABILITY REQUIREMENTS, p. 19

6.1—General, p. 19

6.2—Materials, p. 19

6.3—Steel properties for design, p. 19

6.4—Durability requirements, p. 19

CHAPTER 7—LOADS, p. 20

7.1—General, p. 20

7.2—Dead load, p. 20

7.3—Temperature gradient load, p. 20

7.4—Wind load, p. 23

7.5—Earthquake load, p. 29

7.6—Load combinations, p. 33

CHAPTER 8—DESIGN OF HORIZONTAL CROSS SECTIONS, p. 35

8.1—General, p. 35

8.2—Design limits, p. 36

8.3—Required strength, p. 38

8.4—Design strength, p. 38

8.5—Reinforcement limits, p. 39

8.6—Reinforcement detailing, p. 40

CHAPTER 9—DESIGN OF VERTICAL CROSS SECTIONS FOR CIRCUMFERENTIAL RING MOMENTS, p. 42

9.1—General, p. 42

9.2—Design limits, p. 42

9.3—Required strength, p. 42

9.4—Design strength, p. 42

9.5—Reinforcement limits, p. 43

9.6—Reinforcement detailing, p. 43

CHAPTER 10—OPENING DETAILS, p. 45

10.1—General, p. 45

10.2—Minimum wall thickness at openings, p. 45

10.3—Vertical reinforcement at openings, p. 45

10.4—Circumferential reinforcement at openings, p. 46

10.5—Corner reinforcement at openings, p. 47

10.6—Seismic detailing, p. 48

CHAPTER 11—FOUNDATION, p. 49

11.1—Foundation geotechnical capacity, p. 49

11.2—Foundation structural design, p. 49

11.3—Reinforcement detailing, p. 50

11.4—Mass concrete, p. 50

CHAPTER 12—CONSTRUCTION REQUIREMENTS, p. 51

12.1—General, p. 51

12.2—Concrete strength, p. 51

12.3—Concrete strength tests, p. 51

12.4—Formwork, p. 51

12.5—Concrete placement, p. 52

12.6—Concrete curing, p. 52

12.7—Reinforcement placement, p. 52

12.8—Construction tolerances, p. 53

12.9—Precast erection, p. 53

COMMENTARY REFERENCES, p. 54

APPENDIX A—HORIZONTAL CROSS-SECTION STRENGTH FOR CIRCULAR CHIMNEYS BY MODIFIED STRESS BLOCK METHOD, p. 56

A.1—Notation, p. 56

A.2—Procedure for computing combined nominal axial and flexural strength, p. 56

A.3—Stress block modification factor, p. 58

A.4—Derivation of equations, p. 58

APPENDIX B—HORIZONTAL CROSS-SECTION STRENGTH FOR CIRCULAR CHIMNEYS BY STRESS-STRAIN RELATIONSHIP INTEGRATION METHOD, p. 62

B.1—Notation, p. 62

B.2—Procedure for computing combined nominal axial and flexural strength, p. 62

B.3—Derivation of equations, p. 63

APPENDIX C—TEMPERATURE GRADIENTS FOR CIRCULAR CHIMNEYS, p. 67

C.1—General, p. 67

C.2—Notation, p. 67

C.3—Unlined chimney, p. 67

C.4—Chimney with lining material applied directly to the inside concrete surface, p. 67

C.5—Chimney with insulation completely filling the space between the liner and the chimney wall (no annular airspace), p. 68

C.6—Chimney with unventilated air space between liner and chimney wall, p. 68

C.7—Chimney with ventilated air space between liner and chimney wall, p. 69

APPENDIX D—THERMAL STRESSES FOR CIRCULAR CHIMNEYS, p. 70

D.1—General, p. 70

D.2—Notation, p. 70

D.3—Vertical thermal stresses, p. 70

D.4—Horizontal thermal stresses, p. 70

APPENDIX E—CRACKING MOMENT, p. 72

E.1—Notation, p. 72

E.2—Cracking moment calculation, p. 72

APPENDIX F—REVISION HISTORY, p. 73

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).