ACI PRC-242-22: Alkali-Activated Cements—Report

ACI PRC-242-22: Alkali-Activated Cements—Report

Price: $ 95.00 USD

Choose Product Language

Choose Product Units


Choose Product Format

Description

This report provides a technical overview of alkali-activated cement (AAC) history; chemistry; and mechanical, physical, and durability properties. It also highlights successful case study applications and current technical challenges.

Keywords:

alkali-activated cements (AACs); alternative cements; geopolymers

 

Document Details

Author: ACI Committee 242

Publication Year: 2022

Pages: 20

ISBN: 9781641952002

Categories: Codes

Formats: Printed Document or Protected PDF/Web View

Table of Contents

CHAPTER 1—INTRODUCTION AND SCOPE, p. 2

1.1—Introduction, p. 2

1.2—Scope, p. 2

CHAPTER 2—DEFINITIONS, p. 2

CHAPTER 3—Alkali-activated cement HISTORY, p. 3

CHAPTER 4—Alkali-activated cement TECHNOLOGY AND MIXTURE PROPORTIONING, p. 3

4.1—Alkali-activated cement technology, p. 3

4.2—Mixture proportioning, p. 3

CHAPTER 5—alkali-activated cement PROPERTIES AND PERFORMANCE, p. 5

5.1—Fresh-state properties, p. 5

5.2—Mechanical properties, p. 5

5.3—Durability, p. 6

CHAPTER 6—alkali-activated cement CHALLENGES AND OPPORTUNITIES, p. 8

6.1—Drying and autogenous shrinkage, p. 8

6.2—Durability, p. 9

6.3—Environmental impact, p. 9

CHAPTER 7—alkali-activated cement APPLICATIONS, p. 10

Authored documents, p. 11

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).