ACI PRC-225.2-25: Type IL Cements and Specifications—TechNote

Price: $ 19.00 USD

Choose Product Language

Choose Product Units


Choose Product Format

Description

Type IL (pronounced “one-el”) portland-limestone cements were introduced in ASTM C595/C595M and AASHTO M 240 standard specifications for blended cements in 2012. These cements contain between 5 and 15% limestone, compared to the 5% maximum limestone content of ASTM C150/AASHTO M 85 portland cements. Type IL cements perform comparably to portland cements and do so with up to 10% lower CO2 emissions per ton of cement. Although portland-limestone cements have been available in other parts of the world, the availability and adoption of these cements in practice have only recently become widespread in the United States (as of 2022) (Schexnayder 2022). Many specifiers may have limited experience in incorporating these cements into project specifications.

Keywords:

heat of hydration; high early strength; low-carbon concrete; mixture design; portland-limestone cements; specifications; sulfate resistance.

 

Document Details

Author: ACI Committee 225

Publication Year: 2025

Pages: 4

ISBN:

Table of Contents

Introduction

Question

Answer

Discussion

Summary

References

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).