What conditions suggest the application of internally cured concrete? What are the expected benefits of internal curing using prewetted fine lightweight aggregate?

Keywords:

autogenous volume change; curing; drying shrinkage; early age; fine aggregate; hydration; internal curing; lightweight aggregate; shrinkage; shrinkage cracking.

 

Document Details

Author: ACI Committee 213

Publication Year: 2024

Pages: 5

ISBN:

Categories: Codes

Formats: Protected PDF/Web View

Table of Contents

Question

Answer

Introduction

Discussion

Conditions that suggest internal curing

Expected benefits of internal curing

Conclusions

References

Authored documents

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).