On-Demand Course: A Practical Approach to Designing, Placing, and Protecting Mass Concrete

Currency Display

Your Price: $ 39.00 USD

Member Price: $ 29.00 USD

Save $ 10.00 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Quantity:


Notes/Preview

INSTRUCTIONS: View the recorded webinar. Complete 10-question quiz with a score of 80% or higher to receive a certificate for 0.1 CEU (equivalent to 1.0 PDH).

Continuing Education Credit: 0.1 CEU (1.0 PDH)

Approved by AIA and ICC

Access Period: 30 days

Description

This is a recorded webinar series from June 6, 2017.

When most people think of mass concrete, the first things that come to mind are large dam projects, such as the Hoover Dam that borders both Arizona and Nevada, and other Corps of Engineer dam projects built in the 1930s through the 1960s. In fact, most of the information contained in ACI 207.1R-05 (2012), “Guide to Mass Concrete,” was derived for, and from, these types of projects. However, projects such as wastewater treatment vaults with thickened floor slabs, large mat foundations, pile caps for drilled piers, and large inertia mass machine foundations may require different approaches for mass concrete placements that extend beyond ACI 207.1. This webinar will discuss methods of designing, placing, and protecting mass concrete and realistic thermal-control plans. Examples of actual jobs and field studies will be included in this session.

 

Document Details

Author: McPherson

Publication Year: 2017

ISBN:

Categories: Mass Concrete

Formats: Online Learning

Table of Contents

Learning Objectives

1. Explain the practical concept for Massive Structural Concrete:“Can’t keep it cool? Keep it warm,” an alternative approach to designing, placing, and protecting mass concrete structures.

2. Identify measures taken to ensure internal maximum temperature is no more than 35°F (∆T) greater than the external temperature.

3. Describe how to place a hard trowel finish on the surface of a low-heat, slow-setting mass concrete mixture in a cold environment.

4. Discuss how long it takes for heat to dissipate from a mass structure.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.