Description

This volume deals with dynamic deflections of concrete structures. The collection of 12 papers leads off with a review of the state of the art. Other subjects include: vibration criteria for long-span concrete floors, dynamic characteristics of reinforced concrete buildings, estimation of dynamic stressing of floors and buildings due to shocks and blasting, frequency matching in continuous post-tensioned bridges, dynamic sway characteristics of structures, dynamic response of noncomposite metal deck floor system, concrete structures and construction vibrations, prediction of damage to low-rise buildings due to vibrations created by blasting, vibration performance of industrial buildings. A bibliography is included.

 

Document Details

Publication Year: 1979

ISBN:

Categories: Sustainability

Formats: PDF

Table of Contents

Introduction and Background: Vibrations of Concrete Structures

Deflection Requirements-History and Background Related to Vibrations

Development of Model Performance Criteria for Deflection of Concrete Floors

Vibration Criteria for Long-Span Concrete Floors

Dynamic Characteristics of Reinforced Concrete Buildings

Estimation of the Dynamic Stressing of Floors and Other Structural Parts of Buildings Due to Shocks and Blasting: Determination of Stresses by Measurement of the Vibration Velocity

Frequency Matching in Continuous Post-Tensioned Concrete Highway Bridges

Some Observations on the Dynamic Sway Characteristics of Concrete Structures

Dynamic Response of a Noncomposite Metal Deck Floor System

Concrete Structures and Construction Vibrations

Predictions of Damage to Low-Rise Buildings Due to Ground Vibrations Created by Blastings

Vibration Performance of Industrial Structures

Bibliography on Vibrations of Concrete Structures

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.