SP-041: Fatigue of Concrete

SP-041: Fatigue of Concrete

Currency Display

Your Price: $ 69.50 USD

Member Price: $ 39.00 USD

Save $ 30.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Note: The individual papers are also available as .pdf downloads. Please click on the following link to view the papers available, or call 248.848.3800 to order.

PURCHASE INDIVIDUAL PAPERS


Description

Covers the effects of age, moisture, condition, and the rate of loading on the fatigue of strength of plain concrete. Includes research reports on fatigue properties of rebar, welded wire fabric, and reinforced concrete.

 

Document Details

Publication Year: 1974

ISBN:

Categories: Fatigue

Formats: PDF

Table of Contents

Strength and Deformation Characteristics of Plain Concrete Subjected to High Repeated and Sustained Loads

Effects of Moisture Condition Age, and Rate of Loading on Fatigue of Plain Concrete

Contribution to the Fatigue Strength of Reinforced Concrete

Fatigue of Concrete Under Lateral Confining Pressure

Investigation of Design Factors Affecting Fatigue Strength of Reinforcing Bars-Test Program

Investigation of Design Factors Affecting Fatigue Strength of Reinforcing Bars-Statistical Analysis

Effect of Surface Characteristics on Fatigue Strength of Reinforcing Steel

Stress Concentrations Caused by Reinforcing Bar Deformations

Fatigue Characteristics of Welded Wire Fabric

Fatigue Characteristics in Bond and Shear of Reinforced Concrete Beams

Fatigue Resistance of Under-Reinforced Prestressed Beams Subjected to Different Stress Ranges; Miner's Hypothesis

Behavior of Under-Reinforced Prestressed Concrete Beams Subjected to Different Stress Ranges

Fatigue of Reinforcement in Beams with Limited Prestress

Fatigue Strength of Concrete Slabs Reinforced With Wire Fabric

Are Composite Bridge Slabs Too Conservatively Designed? - Fatigue Studies

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.