SP-335: Nanotechnology for Improved Concrete Performance

Price: $ 69.50 USD

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Sponsors & Editors: ACI Committee 241, Nanotechnology of Concrete, Mahmoud Reda Taha and Mohamed T. Bassuoni

Preview

PURCHASE INDIVIDUAL PAPERS


Description

Many of the papers presented in this volume were included in the two-part session Nanotechnology for Improved Concrete Performance, sponsored by ACI Committee 241, Nanotechnology of Concrete at the ACI Convention in Philadelphia, PA, on October 26, 2016. In line with the practice and requirements of the American Concrete Institute, peer review, followed by appropriate response and revision by authors, has been implemented.

 

Document Details

Pages: 152

ISBN: 9781641950763

Categories: Concrete Technology, Fiber-Reinforced Concrete, Materials

Formats: PDF

Table of Contents

SP-335-1:

Multi-Scale Fiber Reinforcement for Cracking Resistance in Cement Mortars (1-11)

Authors: Joshua Hogancamp, Cesario Tavares, and Zachary Grasley

SP-335-2:

Tailoring The Piezoresistive Sensing of CNT Reinforced Mortar Sensors (12-26)

Authors: Maria S. Konsta-Gdoutos, Panagiotis A. Danoglidis, and Surendra P. Shah

SP-335-3:

Performance of Fiber-Reinforced Carbon Nanotubes-Nanofibers Composites (27-36)

Authors: Joshua Hoheneder, Ismael Flores-Vivian and Konstantin Sobolev

SP-335-4:

Investigation Methods for Characterizing Nanoparticles in Concrete (37-48)

Authors: Douglas Hendrix, Nabil Bassim, and Kay Wille

SP-335-5:

Prediction of Effective Properties of Fly Ash-Based Geopolymers (49-62)

Authors: Sumanta Das, Pu Yang, Sudhanshu S. Singh, James C.E. Mertens, Xianghui Xiao, Nikhilesh Chawla and Narayanan Neithalath

SP-336-6:

Strength Recovery Through Nanosilica Coated Polypropylene Fiber Reinforcement (63-82)

Authors: Su-Jin Lee, Shiho Kawashima, and Jong-Pil Won

SP-335-7:

Hydration and Strength of Cement Pastes Containing Different Nanoparticles (83-96)

Authors: Xin Wang and Kejin Wang

SP-335-8:

Titania and Silica Nanoparticle-Modified Coatings for Cementitious Materials (97-111)

Authors: Qingxu Jin, Marisol Faraldos, Ana Bahamonde, Behnaz H. Zaribaf, and Kimberly E. Kurtis

SP-335-9:

Nano-Modified Concrete Cast and Cured at Freezing Temperature (112-127)

Authors: A. M. Yasien, A. Abayou, and M. T. Bassuoni

SP-335-10:

Evolution of Elastic Modulus and Creep of Nanoclay Modified Oil Well Cement (128-144)

Authors: Vemuganti, S., Rahman, M.K., and Reda Taha, M. M.

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.