SP-178: Sixth CANMET/ACI/JCI Conference: FLy Ash, Silica Fume, Slag & Natural Pozzolans in Concrete

SP-178: Sixth CANMET/ACI/JCI Conference: FLy Ash, Silica Fume, Slag & Natural Pozzolans in Concrete

Price: $ 124.50 USD

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Note: The individual papers are also available as .pdf downloads. Please click on the following link to view the papers available, or call 248.848.3800 to order.

PURCHASE INDIVIDUAL PAPERS

Editor: V.M.Malhotra

Description

This Symposium Publication contains the proceedings of the Fourth CANMET/ACI/JCI International Conference held in Tokushima, Japan, in June 1998. Sixty-two refereed papers were accepted for presentation at this conference and for this publication.

 

Document Details

Publication Year: 1998

Pages: 1154

ISBN: 9780870316777

Categories: Pozzolans

Formats: PDF

Table of Contents

Volume I:

Preface by V.M. Malhotra

Role of Pozzolanic & Cementitious Material in Sustainable

Development of the Concree Industry by P. Kumar Mehta

The Use of Classified Fly Ash to Produce High Performance

Concrete by K.E. Hassan & J.G. Cabrera

Selective Use of Fly Ash Concrete by V. Sirivivatnanon &

R.P. Khatri

Influence of Temperature on Strength Development of Fly

Ash & Silica Fume Concretes by H. Saricimen,

M. Maslehuddin & O.A. Eid

Technological Complex for Utilization of High-Calicum Ash &

Slag for Abakan Thermal Power Plant by S. Pavlenko, A.

Shishkanov & Yu Bazhenov

Comparative Study on Mortar Containing Fly Ash From

Southeast Asia & Japan in Relation to Strength & Durability

by K. Wangwichit, M. Hisada, N. Otsuki & S. Nagataki

Significance of the Thype of Cement on the Reaction

Mechanisms of Pozzolans by B. Meng, U. Wiens & P.

Schiessl

A Comparison of Mechanical Properties of Hong Kong

Medium & High-Strenght NPC & Fly Ash Concretes by

I.D. MacGregor

Highly Flowable Steel Fiber-Reinforced Concrete

Containing Fly Ash by M. Kurita & T. Nomura

Effect of Steam Curing on Compressive Strength of Fly

Ash Concrete by K. Kohno, Y. Mitsuiwa & K. Ishimaru

The Chemical Shrinkage of Pozzolanic Reaction Products by

H. Justnes, B. Ardoullie, E. Hendrix, E.J. Sellevold & D. Van

Gemert

Microstructural Study of Hydration Reactions of a Fly-Ash

Belite Cement by S. Goni, M.P. Luxan, A. Guerrero, M.S.

Hernandez & A. Macias

A Novel Clinkerization Process for Fly-Ash Utilization by

S.A. Khandilkar, M.V. Karandikar, D. Ghosh & A.K. Chatterjee

Fly Ash Customization for Defined Performance Concretes

by H.A.W. Cornelissen & J.W. van den Berg

Influence of Unburnt Carbon in the Performance of Concrete

Mixtures bu L. Coppola, R. Troli, P. Zaffaroni, G. Belz &

M. Collepardi

Durability Study of Mount Pinatubo Ejecta Concrete Paving

Blocks by J.G. Agron

Optimized Solidification of Mixtures of MSWI Fly Ash & Blast

Furnace Slag: Use of the Statistical Design of Experiments

by S. Morel, P. CLastres, D. Mathieu & A. Pellequer

Effects of Fly Ash & Silica Fume on High Performance

Concrete by S. Nagataki, S. Miyazato & T. Saitoh

Engineering Properties of High Volume Fly Ash Concrete

by R.N. Swamy & H.H. Hung

Effect of Curing Methods & Conditions on the Performance

of Fly Ash Concrete in De-Icing Salt Scaling by A. Bilodeau,

M.H. Zhang, V.M. Malhotra & D.M. Golden

The Microstructure & Chloride Ion Diffusion Characteristics

of Cements Containing Metakaolin & Fly Ash by J.G.

Cabrera & S.O. Nwaubani

Effects of Fine Aggregate Replacement on the Rheology,

Compressive Strength & Carbonation Properties of Fly Ash

& Mortar by K.R. Hwang, T. Noguchi & F. Tomosawa

Slump Loss: A Single Rule for Ordinary Concrete by B. Pollet,

R. Lavaud & J. Baron

*Influence of Palm Oil Fuel Ash on Sulfate Resistance of

Mortar & Concrete by M. Warid Hussin & A.S.M. Abdul Awal

Mineralogical & Chemical Properties of Mortar Incorporating

Coal Ash Produced by Fluidized Bed Combustion by

N. Shintani, T. Saitou, H. Sasaki & T. Kita

Mechanical Properties & Durability of Structural Lightweight

Concrete Incorporating High Volumes of Fly Ash by A.

Bilodeau, V.M. Malhotra & D.M. Golden

*Supplementary Cementing Materials: Their Acceptance in

Australian Specification by D. Baweja & P. Nelson

De-Icing Salt Scaling of Concrete Incorporating Different

Types & Percentages of Fly Ash by M.H. Zhang, A. Bilodeau,

G. Shen & V.M. Malhotra

Utilization of Coal Ash Produced From Pressurized Fluidized

Bed Combustion Power Plant as a Concree Mineral Admixture

by K. Fukudome, N. Shintani, T. Saitoh, T. Kita & H. Sasaki

Practical Uses for High-Volume Fly Ash Concrete Using a Low

Calcium Fly Ash by W.S. Langley & G.H. Leaman

Mechanical Properties & Durability of Concrete Made With

High Volume Fly Ash Blended Cements by N. Bouzoubaa,

M.H. Zhang, A. Bilodeau & V.M. Malhotra

Volume II:

Preface by V. M. Malhotra

The Repair of High-Strength Silica Fume Concrete: A Case

History by G.C. Hoff & R. Elimov

Pozzolanic Interaction Between Portland Cement & Silica

Fume in Concrete by B.S.M. Persson

Engineering Properties of Concretes With Combinations

of Cementitious Materials by R.N. Swamy & A.A. Darwish

The Influence of Physical Properties of Aggregate on

Shrinkage on High Strength Slag Cement Concrete by

H. Matsushita, H. Tsuruta & K. Nakae

Chloride Penetration Into Concretes Incorporating Mineral

Admixtures in Marine Environment by K. Torii, T. Sasatani

& M. Kawamura

Performance of Blast Furnace Slag Cement Concrete in

Simulated Aggressive Marine Environment by K. Torii,

& K. van Bruegel

High Strength Natural Lightweight Aggregate Concrete

With Silica Fume by A. Yeginobali, K.G. Sobolev, S.V.

Soboleva & M. Tokyay

Performance of a Different Pozzolanic Cement Concrete

Under Cyclic Wetting & Drying by A.A. Ramezanianpour,

Radfar, Hadikhanloo, Moslehi & Maghsoodi

Water Permeability of High Slag Content Concrete by

J. Nakamoto, K. Togawa, T. Miyagawa & M. Fujii

Effect & Mechanism of Natural Zeolite on Supressing

ASR in Concrete by N. Feng, H. Jia & T. Hao

Monitoring Hydration of Alkali-Activated Slag & Fly Ash

by H.C. Ezirim & W.J. McCarter

Studies on the Properties of Super Workable Concrete

Using Ground Granulated Blast-Furnace Slag by Y. Madea,

T. Chikada, Y. Nagao, Y. Dan & H. Matsushita

Compressive Strength of Portland Blast Furnace Slag

Cement Concrete in Adiabatic & Semi-Temperature

Matched Curing Conditions by J.L. Yang, E.Y. Chen, G.L.

Low & B.T. Tan

Pore Atructure, Strength & Carbonation of Cement Pastes

Containing Ground Granulated Blast-Furnace Slag by

C. Li, A. Yoda & T. Yokomuro

Potential of Blast Furnace Slags to Immobilize Toxic

Wastes by A. Macias, S. Goni, J. Madrid, J.M. Diez

& E. del Castillo

Effect of Superplasticizers in Highly Alkaline Model

Suspensions Containing Silica Fume by R.J. Flatt,

Y.F. Houst, P. Bowen, H, Hofmann, J. Widmer, U. Sulser,

U. Maeder & T.A. Burge

Silica Fume Distribution & Reactivity in Reactive Powder

Concretes by L. Gatty, S. Bonnamy, A. Feylessoufi, H. Van

Damme & P. Richard

Microstructures of Concretes Made With & Without Blast

Furnace Slag After 40 Yrs of Immersion in Saturated

Gypsum Solutions at 20 C by A.C. Courault, A.K.

Crumbie, D. Sorrentino & D. Damidot

Influence of Silica Fume on Permeability of Concrete to

Oxygen for Temperatures up to 500 C by M.S. Zadeh,

G. Debicki, P. Clastres & Y. Billard

Immobilization of Wastes by Metakaolin-Blende Cements

by J. Pera, E. Bonnin & M. Chabannet

Pozzolanic Properties of Metakaolin Obtained From

Paper Sludge by J. Pera & J. Ambroise

Using natural Pozzolans to Improve the Sulfate Resistance

of Cement Mortars by R.E. Rodriguez-Camacho

Suitability of Fumed Lead Blast-Furnace Slag as a

Mineral Admixture for Concrete by D.L. Thomas, M.D.A.

Thomas & J. Ryell

Soil Stabilization Using Lime-Activated Ground Granulated

Blast Furnace Slag by D.D. Higgins, J.M. Kinuthia & S.Wild

Limestone Modified Cement for High-Performance Concretes

by D.G. Montgomery, B.K. Van, I. Hinczak & K. Turner

Chemical Development of the Fluid From Pores of Admixture

Bearing Mortars Affected by the Alkali-Aggregate Reaction

by J.D. Sota, R. Iasi, R. Perez & O.R. Batic

High Calcium Fly Ash - To Silica Fume - To Slag Sand

Ratio Versus Compressive Strength & Density of

Cementless Concrete by S.I. Pavlenko, L.P. Myshlyaev,

V.F. Evtushenko, A.V. Soin & Yu M. Bazhenov

Influence of Storage Conditions & Concrete Composition

on the Effictiveness of Different Silica Fumes Against ASR

by M.A. Berube, J. Duchesne & J. Frenette

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).