E-1(16) Aggregates for Concrete

Currency Display

Your Price:$ 0.00 USD

Member Price: $ 0.00 USD

Choose download Format

Description

Aggregate properties and gradation significantly affect workability and finishability of freshly placed concrete and properties of hardened concrete including compressive strength, durability and abrasion resistance. Properties and accepted test methods discussed in this bulletin include: aggregate gradation; fine and coarse aggregate fineness moduli; relative bulk densities of wet, saturated surface dry, air-dry, and oven-dry aggregates; moisture absorption; shape angularity and surface texture; abrasion and impact resistance; permeability resistance to freeze thaw cycles and alkali-silica reaction; and chemical stability. Aggregate types including normalweight, lightweight and heavyweight natural aggregate; blast furnace slag aggregates; and recycled aggregates from crushed reclaimed concrete pavements are covered. Examples are provided on how to calculate and evaluate fineness modulus, batch mixture proportions adjusted for aggregate absorption, batch mixing water proportions, water cementitious ratios and bulk densities. Sampling aggregate methods to estimate average aggregate properties of large volumes or stockpiles, batches, or truckloads of aggregates are also covered.

Keywords: abrasion resistance, absorption, aggregate angularity, aggregate gradation, aggregate surface texture, air-dry bulk density, alkali-silica reaction, batch mixture proportioning, blast-furnace slag aggregate, bulk density, compaction, fineness modulus, heavyweight aggregate, lightweight aggregate, mixing water, normalweight aggregate, oven-dry bulk density, recycled aggregate, relative bulk density, saturated surface-dry bulk density, sampling, surface moisture, water-cementitious ratio.

 

Document Details

Author: ACI Committee E701

Publication Year: 2016

Pages: 26

ISBN: 9781942727750

Categories: Aggregates

Formats: PDF, ePub, or Kindle

Table of Contents

CHAPTER 1—INTRODUCTION

CHAPTER 2—CLASSIFICATION OF AGGREGATES

CHAPTER 3—AGGREGATE PROPERTIES AND TEST METHODS

3.1—Grading

3.2—Relative density (specific gravity)

3.3—Absorption and surface moisture

3.4—Bulk density

3.5—Particle shape and surface texture

3.6—Abrasion and impact resistance

3.7—Soundness

3.8—Chemical stability

3.9—Harmful substances

CHAPTER 4—SAMPLING AGGREGATES

4.1—Variability in aggregates

4.2—Sampling

CHAPTER 5—BLAST-FURNACE SLAG AND LIGHTWEIGHT AGGREGATES

5.1—Blast-furnace slag

5.2—Lightweight aggregates

5.3—Recycled aggregates

CHAPTER 6—REFERENCES

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.