This guide provides technical information on physical and mechanical properties, design criteria, and testing of ferrocement. The objectives are to promote the most effective use of ferrocement in terrestrial structures, provide architects and engineers with the necessary tools to specify and use ferrocement, and provide owners or their representatives with a reference document to check the acceptability of a ferrocement alternative in a given application.

Keywords: composite materials; construction materials; ferrocement; fibers; reinforcing materials; structural design; welded wire fabric.

 

Document Details

Author: ACI Committee 549

Publication Year: 2018

Pages: 28

ISBN: 9781641950329

Categories: Fiber-Reinforced Concrete

Formats: PDF

Table of Contents

CHAPTER 1—GENERAL

1.1—Scope

1.2—Approval for use in design and construction

CHAPTER 2—NOTATION AND DEFINITIONS

2.1—Notation

2.2—Definitions

CHAPTER 3—PHYSICAL AND MECHANICAL PROPERTIES

3.1—Introduction

3.2—Reinforcing parameters

3.3—Ultimate strength under static load

3.4—First-crack strength under static load

3.5—Elasticity and load-deformation behavior

3.6—Strength under fatigue loading

3.7—Impact resistance

3.8—Crack development and leakage

3.9—Shrinkage and creep

3.10—Durability

3.11—Fire resistance

CHAPTER 4—PERFORMANCE CRITERIA

4.1—Introduction

4.2—Design methods

4.3—Allowable tensile stress

4.4—Allowable compressive stress

4.5—Volume fraction and specific surface of reinforcement

4.6—Cover requirements

4.7—Crack width limitations

4.8—Stress range

CHAPTER 5—DESIGN CRITERIA

5.1—Design methods

5.2—Strength requirements

5.3—Service load design

5.4—Serviceability

5.5—Particular design parameters

5.6—Examples

5.7—Design aids

CHAPTER 6—TESTING

6.1—Test methods

CHAPTER 7—REFERENCES

Authored documents

APPENDIX A—CALCULATION OF VOLUME FRACTION OF REINFORCEMENT

APPENDIX B—FLEXURAL STRENGTH ANALYSIS OF FERROCEMENT SECTIONS

APPENDIX C—SIMPLIFIED DESIGN AIDS

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.