Description

This Specification covers epoxy slurry (ES) polymer overlay for bridge and parking garage decks. Type ES polymer overlay incorporates a low-modulus epoxy binder, fillers, and selected aggregate to produce a flexible, skid-resistant, and low-permeability overlay. The overlay may be used for both new construction and rehabilitation of existing structures. The overlay is placed by applying the mixed epoxy binder and filler to the surface and broadcasting aggregate. This Specification includes requirements for epoxy resin, fillers, aggregates, storage and handling, surface preparation, surface profile, mixing, placement, quality control, and quality assurance.

Keywords:

bridge decks; epoxy; low permeability; parking garage decks; polymer overlay; slurry; surface preparation.

 

Document Details

Author: ACI Committee 548

Publication Year: 2022

Pages: 6

Categories: Codes

Formats: Protected PDF/Web View

Table of Contents

PART 1—GENERAL, p. 2

1.1—Scope, p. 2

1.2—Interpretation, p. 2

1.3—Definitions, p. 2

1.4—Reference standards, p. 3

1.5—Submittals, p. 3

1.6—Project conditions, p. 3

1.7—Delivery, storage, and handling of materials, p. 3

1.8—Safety, p. 3

1.9—Quality assurance, p. 3

PART 2—PRODUCTS, p. 3

2.1—Epoxy binder, p. 3

2.2—Fillers, p. 4

2.3—Aggregate, p. 4

2.4—Polymer overlay, p. 4

PART 3—EXECUTION, p. 4

3.1—Procedure qualification, p. 4

3.2—Surface preparation, p. 5

3.3—Mixing epoxy primer and slurry, p. 5

3.4—Overlay application, p. 5

3.5—Curing, p. 5

3.6—Excess aggregate removal, p. 5

3.7—Joints, p. 5

3.8—Open to traffic, p. 5

NOTES TO SPECIFIER, p. 5

General notes, p. 5

Foreword to checklists, p. 6

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).