ACI SPEC-548.8-19: Construction Specification for Type EM (Epoxy Multi-Layer) Polymer Overlay for Bridge and Parking Garage Decks

Currency Display

Your Price:$ 54.50 USD

Member Price: $ 34.00 USD

Save $ 20.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Notes/Preview

Preview

Description

This Specification covers epoxy multi-layer (EM) polymer overlay for bridge and parking garage decks. Type EM polymer overlay incorporates a low-modulus epoxy binder and selected aggregate to produce a flexible, skid-resistant, and low-permeability overlay. The overlay may be used for both new construction and rehabilitation of existing structures. The overlay is placed by applying the neat epoxy binder to the surface and broadcasting aggregate. This Specification includes requirements for epoxy resin, aggregates, storage and handling, surface preparation, surface profile, mixing, placement, quality control and quality assurance.

Keywords: bridge decks; epoxy; multi-layer; parking garage decks; polymer overlay; surface preparation; low permeability.

 

Document Details

Author: ACI Committee 548

Pages: 8

Categories: Polymer Concrete

Formats: PDF

Table of Contents

SECTION 1—GENERAL

1.1—Scope

1.2—Interpretation

1.3—Definitions

1.4—Reference standards

1.5—Submittals

1.6—Project conditions

1.7—Labeling, storage, and handling of materials

1.8—Quality assurance and quality control acceptance of work

SECTION 2—PRODUCTS

2.1—Epoxy binder

2.2—Aggregate

SECTION 3—EXECUTION

3.1—Procedure qualification

3.2—Surface preparation

3.3—Mixing epoxy binder

3.4—Overlay application

3.5—Curing

3.6—Excess aggregate removal

3.7—Joints

3.8—Open to traffic

NOTES TO SPECIFIER (nonmandatory)

General notes

Foreword to checklists

MANDATORY REQUIREMENTS CHECKLIST

SUBMITTAL CHECKLIST

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.