ACI SPEC-548.15-20: Specification for Crack Repair by Epoxy Injection

ACI SPEC-548.15-20: Specification for Crack Repair by Epoxy Injection

Currency Display

Your Price:$ 59.00 USD

Member Price: $ 35.00 USD

Save $ 24.00 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Description

This Specification gives requirements for repairing cracks in concrete by injection of two-component epoxy-resin adhesive.

Keywords:

adhesive; crack; epoxy; repair injection; sealer.

 

Document Details

Author: ACI Committee 548

Publication Year: 2021

Pages: 8

ISBN:

Categories: Codes

Formats: Printed Document or Protected PDF/Web View

Table of Contents

PART 1—GENERAL, p. 2

1.1—Scope, p. 2

1.2—Interpretation, p. 2

1.3—Definitions, p. 2

1.4—Reference standards, p. 3

1.5—Submittals, p. 3

1.6—Delivery, storage, and handling, p. 3

1.7—Quality assurance and quality control acceptance of work, p. 3

PART 2—PRODUCTS, p. 5

2.1—Surface seal, p. 5

2.2—Injection adhesives, p. 5

PART 3—EXECUTION, p. 5

3.1—Evaluation and preparation, p. 5

3.2—Test injection, p. 5

3.3—Injection, p. 5

3.4—Cleanup, p. 6

3.5—Safety, p. 6

NOTES TO SPECIFIER (NONMANDATORY), p. 6

General notes, p. 6

Foreword to Checklists, p. 6

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).