ACI SPEC-548.14-14 Specification for Repairing Concrete with Epoxy Mortar

ACI SPEC-548.14-14 Specification for Repairing Concrete with Epoxy Mortar

Currency Display

Your Price:$ 42.50 USD

Member Price: $ 28.00 USD

Save $ 14.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

Preview

**A newer version of this document exists**

NEW VERSION

 

Description

This specification describes the work of repairing defects in hardened portland cement concrete with an epoxy mortar. Included are controls for epoxy resin system labeling, storage, handling, surface evaluation and preparation, mixing and application, inspection, quality control, and testing.

Keywords: adhesion to concrete; aggregate; concrete construction; epoxy; hardened concrete; epoxy mortar; quality control; repairs; resurfacing.

 

Document Details

Author: ACI Committee 548

Publication Year: 2015

Pages: 5

Categories: Polymer Concrete

Formats: PDF, ePub, or Kindle

This document is Historical

Table of Contents

PART 1—GENERAL

1.1—Scope

1.2—Interpretation

1.3—Definitions

1.4—Referenced standards

1.5—Submittals

1.6—Product delivery, storage, and handling

1.7—Project conditions

PART 2—PRODUCTS

2.1—Materials

PART 3—EXECUTION

3.1—Preparation

3.2—Inspection of surface prior to epoxy mortar application

3.3—Epoxy mortar mixtures

3.4—Epoxy mortar application

3.5—Field quality control

3.6—Cleanup

3.7—Safety

NOTES TO SPECIFIER

General notes

FOREWORD TO CHECKLISTS

MANDATORY REQUIREMENTS CHECKLIST

OPTIONAL REQUIREMENTS CHECKLIST

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).