ACI SPEC-548.13-21: Multi-Component Epoxy Adhesive for Bonding to Concrete—Specification

ACI SPEC-548.13-21: Multi-Component Epoxy Adhesive for Bonding to Concrete—Specification

Currency Display

Your Price:$ 59.00 USD

Member Price: $ 35.00 USD

Save $ 24.00 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Description

This Specification describes bonding fresh concrete, hardened concrete, steel, and other materials as covered in Section 2.3 to hardened concrete with a multi-component epoxy adhesive as defined for this purpose in ASTM C881/C881M. Included are controls for adhesive labeling; storage; handling; surface evaluation and preparation; mixing and application; and inspection, safety, quality control, and testing.

Keywords:

adhesive; bond; construction; epoxy; epoxy resin; fresh concrete; quality control; repair; safety; surface.

 

Document Details

Author: ACI Committee 548

Publication Year: 2022

Pages: 12

ISBN:

Categories: Codes

Formats: Printed Document or Protected PDF/Web View

Table of Contents

SECTION 1—GENERAL REQUIREMENTS, p. 2

1.1—Scope, p. 2

1.2—Interpretation, p. 2

1.3—Definitions, p. 2

1.4—Referenced standards, p. 3

1.5—Submittals, p. 3

1.6—Delivery, storage, and handling, p. 3

1.7—Project conditions, p. 3

1.8—Control of adhesive mixture, p. 3

SECTION 2—BONDING HARDENED CONCRETE, STEEL, AND OTHER MATERIALS TO HARDENED CONCRETE, p. 3

2.1—General, p. 3

2.2—Products, p. 3

2.3—Execution, p. 4

SECTION 3—BONDING FRESH CONCRETE TO HARDENED CONCRETE, p. 5

3.1—General, p. 5

3.2—Products, p. 5

3.3—Execution, p. 5

NOTES TO SPECIFIER (nonmandatory), p. 6

General notes, p. 6

Foreword to Checklists, p. 6

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).