ACI SPEC-548.10-10 Specification for Type MMS (Methyl Methacrylate Slurry) Polymer Overlays for Bridge and Parking Garage Decks

ACI SPEC-548.10-10 Specification for Type MMS (Methyl Methacrylate Slurry) Polymer Overlays for Bridge and Parking Garage Decks

Currency Display

Your Price:$ 41.50 USD

Member Price: $ 27.00 USD

Save $ 14.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format


Notes/Preview

**A newer version of this document exists**

NEW VERSION

 

Description

This Specification covers methyl methacrylate slurry (MMS) overlays for bridge and parking garage decks. Type MMS polymer overlay incorporates methyl methacrylate-based primer, binder, and top coat with selected filler and aggregate to produce a flexible, skid-resistant, and water-resistant slurry overlay. The overlay is used for both new construction and rehabilitation. The overlay is placed by applying the polymer slurry system to the surface and broadcasting aggregate. This Specification includes requirements for chemical components, aggregates, storage and handling, surface preparation, surface profile, mixing, placement, finishing, and quality control. The materials, processes, quality control measures, and inspections described in this document should be tested, monitored, or performed as applicable only by individuals with appropriate ACI certifications or equivalent.

Keywords: aggregate; bridge decks; methyl methacrylate; mortar; overlays; parking garage decks; polymer; premixed; resin; slurry.

 

Document Details

Author: ACI Committee 548

Publication Year: 2010

Pages: 6

ISBN:

Categories: Polymer Concrete, Specifications

Formats: PDF

This document is Historical

Table of Contents

Section 1—General

1.1—Scope

1.2—Definitions

1.3—Reference standards

1.4—Submittals

1.5—Project conditions

1.6—Labeling, storage, and handling of materials

1.7—Safety

Section 2—Products

2.1—Methyl methacrylate-based primer

2.2—Methyl methacrylate-based binder

2.3—Filler

2.4—Methyl methacrylate-based top coat

2.5—Aggregate

2.6—Polymer overlay slurry

Section 3—Execution

3.1—Procedure qualification

3.2—Surface preparation

3.3—Mixing methyl methacrylate-based primer, binderfiller

slurry, and top coat

3.4—Overlay application

3.5—Curing

3.6—Excess aggregate removal

3.7—Joints

3.8—Opening to traffic

Notes to Specifier

General notes

Foreword to checklists

Mandatory Requirements Checklist

Submittals Checklist

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).