ACI SPEC-522.1-20: Specification for Construction of Pervious Concrete Pavement

ACI SPEC-522.1-20: Specification for Construction of Pervious Concrete Pavement

Currency Display

Your Price:$ 79.50 USD

Member Price: $ 49.00 USD

Save $ 30.50 USD, Become a Member

Choose Product Language

Choose Product Units


Choose Product Format

Description

This Specification covers minimum requirements for the construction of pervious concrete pavement. This Specification covers materials, preparation, forming, lacing, finishing, jointing, curing, and quality control of pervious concrete pavement. Provisions governing testing, evaluation, and acceptance of pervious concrete pavement are included.

Keywords:

construction; curing; inspection; jointing; parking lots; testing

 

Document Details

Author: ACI Committee 522

Pages: 8

ISBN:

Categories: Codes

Formats: Printed Document or Protected PDF/Web View

Table of Contents

(mandatory portion follows)

PART 1—GENERAL, p. 2

1.1—Scope, p. 2

1.2—Interpretation, p. 2

1.3—Definitions, p. 2

1.4—Referenced standards, p. 3

1.5—Submittals, p. 3

1.6—Quality assurance and quality control, p. 3

PART 2—PRODUCTS, p. 4

2.1—Subbase, p. 4

2.2—Pervious concrete, p. 4

2.3—Isolation joint material, p. 5

2.4—Forms, p. 5

2.5—Curing materials, p. 5

PART 3—EXECUTION, p. 5

3.1—Subgrade preparation, p. 5

3.2—Subbase, p. 5

3.3—Setting formwork, p. 5

3.4—Batching, mixing, and delivery, p. 5

3.5—Placing and finishing fixed-form pavement, p. 5

3.6—Placing and finishing slipform pavement, p. 5

3.7—Edging, p. 6

3.8—Final surface texture, p. 6

3.9—Jointing, p. 6

3.10—Curing, p. 6

3.11—Hot or cold weather construction, p. 6

3.12—Tolerances, p. 6

3.13—Opening to traffic, p. 6

NOTES TO SPECIFIER (nonmandatory), p. 6

General notes, p. 6

FOREWORD TO CHECKLISTS, p. 6

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).