ACI PRC-506-22: Shotcrete - Guide

Price: $ 99.00 USD

Choose Product Language

Choose Product Units


Choose Product Format

Description

This guide is a companion document to ACI 506.2, “Specification for Shotcrete,” and provides information on materials and properties of both dry-mix and wet-mix shotcrete. Most facets of the shotcrete process are covered, including application procedures, equipment requirements, and responsibilities of the shotcrete crew. Other aspects, such as preconstruction trials, craftsman qualification tests, materials tests, finished shotcrete acceptance tests, and equipment, are also discussed.

Keywords:

dry-mix shotcrete; mixture proportioning; placing; quality control; shotcrete; wet-mix shotcrete.

 

Document Details

Author: ACI Committee 506

Publication Year: 2022

Pages: 52

ISBN: 9781641952019

Formats: Printed Document or Protected PDF/Web View

Table of Contents

Contents

PREFACE, p. 2

Introduction, p. 2

History, p. 2

Applications, p. 3

New developments, p. 3

Research and development, p. 3

PART 1—GENERAL, p. 3

1.1—Scope, p. 3

1.2—Definitions, p. 5

1.3—References: Refer to Part 7, p. 5

1.4—Submittals, p. 5

1.5—Preconstruction testing by contractor, p. 5

1.6—Testing during construction: quality assurance and quality control, p. 6

1.7—Acceptance, p. 9

PART 2—PRODUCTS, p. 9

2.1—Materials, p. 9

2.2—Packaged shotcrete materials, p. 13

2.3—Fiber-reinforced shotcrete, p. 13

2.4—Shotcrete properties, p. 13

2.5—Mixture proportions, p. 16

2.6—Batching and mixing, p. 18

PART 3—EXECUTION, p. 20

3.1—Surface preparation, p. 20

3.2—Joints, p. 24

3.3—Alignment control, p. 24

3.4—Application, p. 25

3.5—Finishing, p. 35

3.6—Curing, p. 38

3.7—Protection, p. 38

3.8—Tolerances, p. 38

3.9—Repair, p. 39

PART 4—EQUIPMENT, p. 39

4.1—Introduction, p. 39

4.2—Dry-mix equipment, p. 40

4.3—Wet-mix equipment, p. 41

4.4—Air requirements, p. 42

4.5—Mixing equipment, p. 43

4.6—Hoses, p. 43

4.7—Nozzles, p. 44

4.8—Auxiliary equipment, p. 45

4.9—Plant layout and operation, p. 46

4.10—Other uses of shotcrete equipment, p. 47

PART 5—CREW ORGANIZATION, p. 47

5.1—Introduction, p. 47

5.2—Composition and crew duties, p. 47

5.3—Crew qualifications, p. 48

5.4—Communication, p. 49

PART 6—SUSTAINABILITY, p. 49

6.1—Shotcrete sustainability, p. 49

6.2—Formwork reduction or elimination, p. 49

6.3—Construction efficiency, p. 50

6.4—Repair and rehabilitation, p. 50

6.5—Creativity and efficiency of shotcrete sections, p. 50

6.6—Summary, p. 50

PART 7—REFERENCES, p. 50

Authored references, p. 52

ERRATA INFO

Any applicable errata are included with individual documents at the time of purchase. Errata are not included for collections or sets of documents such as the ACI Collection. For a listing of and access to all product errata, visit the Errata page.

Return/Exchange Policy

Printed / Hard Copy Products: The full and complete returned product will be accepted if returned within 60 days of receipt and in salable condition. A 20% service charge applies. Return shipping fees are the customer’s responsibility.

Electronic /Downloaded Products & Online Learning Courses: These items are not eligible for return.

Subscriptions These items are not eligible for return.

Exchanges: Contact ACI’s Customer Services Department for options (+1.248.848.3800 – ACICustomerService@concrete.org).

Please enter this 5 digit unlock code on the web page.